Nano-Filler Sugarcane Bagasse Ash in Ultra-High-Performance Concrete: A Comprehensive Review of Performance, Mechanisms, and Sustainability

Nano-Filler Sugarcane Bagasse Ash in Ultra-High-Performance Concrete: A Comprehensive Review of Performance, Mechanisms, and Sustainability

ES评分 0

DOI 10.20900/jsr20260057
刊名
JSR
年,卷(期) 2026, 8(2)
作者
作者单位

Civil Engineering Department, Faculty of Engineering, Islamic University of Gaza, P.O. Box 108, Gaza Strip, Palestine Department of Civil Engineering, College of engineering in Al-Kharj, Prince Sattam bin Abdulaziz University, Al-Kharj 11942, Saudi Arabia

摘要
Ultra-high-performance concrete (UHPC) is characterised by exceptional mechanical strength and durability, with compressive strengths commonly exceeding 120 MPa and, in optimised systems, reaching 150–200 MPa. However, this performance is achieved at the expense of high material cost, embodied energy, and environmental impact because conventional UHPC contains very high cementitious contents, typically 1100–1300 kg/m3, and ultra-low water-to-binder ratios of approximately 0.14–0.20. This review critically investigates the integrated performance of sugarcane bagasse ash (SCBA) as a bio-based, silica-rich supplementary cementitious material and nano-/micro-filler in UHPC, focusing on mix design, fresh properties, hydration mechanisms, durability, and sustainability. SCBA has been investigated as a partial cement replacement at approximately 20–40 wt.% and as a quartz powder/filler replacement at approximately 40–60 wt.%, with some studies reporting replacement levels up to 80%, depending on processing quality and fineness. SCBA-modified UHPC has been reported to retain or improve flowability at optimised dosages, with flow diameters of approximately 220–260 mm, while reducing autogenous shrinkage by approximately 19–30%. Mechanical performance can be maintained or improved, with reported compressive strength of approximately 130.8 MPa at 91 days for 40% cement replacement and approximately 136.9 MPa compressive strength and 23.7 MPa flexural strength for 60% quartz powder replacement. Microstructural evidence indicates matrix densification through secondary C–S–H/C–A–S–H formation, pore refinement, internal curing, and improved interfacial transition zone quality. Durability results indicate reduced permeability and chloride-related transport, while sustainability assessments report reductions in global warming potential and material cost. Despite these advantages, variability in SCBA composition, rheological sensitivity, non-standardised processing, and limited field validation remain significant challenges.
Abstract
Ultra-high-performance concrete (UHPC) is characterised by exceptional mechanical strength and durability, with compressive strengths commonly exceeding 120 MPa and, in optimised systems, reaching 150–200 MPa. However, this performance is achieved at the expense of high material cost, embodied energy, and environmental impact because conventional UHPC contains very high cementitious contents, typically 1100–1300 kg/m3, and ultra-low water-to-binder ratios of approximately 0.14–0.20. This review critically investigates the integrated performance of sugarcane bagasse ash (SCBA) as a bio-based, silica-rich supplementary cementitious material and nano-/micro-filler in UHPC, focusing on mix design, fresh properties, hydration mechanisms, durability, and sustainability. SCBA has been investigated as a partial cement replacement at approximately 20–40 wt.% and as a quartz powder/filler replacement at approximately 40–60 wt.%, with some studies reporting replacement levels up to 80%, depending on processing quality and fineness. SCBA-modified UHPC has been reported to retain or improve flowability at optimised dosages, with flow diameters of approximately 220–260 mm, while reducing autogenous shrinkage by approximately 19–30%. Mechanical performance can be maintained or improved, with reported compressive strength of approximately 130.8 MPa at 91 days for 40% cement replacement and approximately 136.9 MPa compressive strength and 23.7 MPa flexural strength for 60% quartz powder replacement. Microstructural evidence indicates matrix densification through secondary C–S–H/C–A–S–H formation, pore refinement, internal curing, and improved interfacial transition zone quality. Durability results indicate reduced permeability and chloride-related transport, while sustainability assessments report reductions in global warming potential and material cost. Despite these advantages, variability in SCBA composition, rheological sensitivity, non-standardised processing, and limited field validation remain significant challenges.
关键词
ultra-high-performance concrete (UHPC); sugarcane bagasse ash (SCBA); supplementary cementitious materials (SCMs); nanoscale pozzolanic reaction; circular economy; microstructural densification; durability performance; sustainable development goals; life-cycle assessment (LCA)
KeyWord
ultra-high-performance concrete (UHPC); sugarcane bagasse ash (SCBA); supplementary cementitious materials (SCMs); nanoscale pozzolanic reaction; circular economy; microstructural densification; durability performance; sustainable development goals; life-cycle assessment (LCA)