| Abstract |
Phenolic resin has the advantages of good adhesion, little influence of temperature and salinity on curing property and dense structure. Water-based phenolic resin and cement have good compatibility, with the potential to improve the property of cement slurry. In this paper, phenolic resin modified cement was studied in view of the problems of brittleness and shrinkage of the traditional cement. The thickening time, mechanical properties, thermal stability and plugging strength of phenolic resin modified cement were evaluated respectively, and the toughening mechanism and action mode of phenolic resin modified cement were clarified. The experimental results show that the initial solidified time of pure cement and cement with 5%, 10% and 15% phenolic resin (referred to as resin cement) is 6, 8, 9, 10 h, respectively, within the safe pumping time of downhole operation in the oil field. The uniaxial compressive strength of pure cement and 5%, 10%, 15% resin cement did not change significantly, while the elastic modulus of 15% resin cement decreased by 57.69%, indicating that resin cement has better deformation ability and impact resistance. With the increase of the proportion of resin, the phenolic resin is evenly distributed in the interior and surface of cement particles after curing, forming a dense three-dimensional network structure, which enhances the toughness of cement and significantly improves the thermal stability of cement. In the 5 mm fracture core, the outlet flow rate of the cement system reaches 354 mL/min at a pressure-bearing of 30 MPa, while the outlet flow rate of the resin cement system is only 98 mL/min. Compared with the pure cement, the pressure-bearing gas-sealing capacity of the resin cement has been greatly improved.
|